Short answer

Silicone wins where heat resistance, food/medical contact and long-term clarity matter; TPU wins where abrasion resistance and tear strength matter; TPE (TPE-S) wins on cost and recyclability but loses on heat and stain resistance. They can look identical on a shelf and fail differently in a dishwasher, a hot car or a baby’s mouth — so decide by the application, not the price.

Silicone vs TPE vs TPUTemperature and application mapping of three elastomers.SiliconeTPUTPE-S-60–200 °Cfood / medical OKstain: excellenttear: moderateclarity: excellentthermoset-40–100 °Cwear surfacestain: goodtear: excellentyellows over timethermoplastic-40–100 °Ccheapstain: poortear: moderateyellows fastthermoplasticAbove ~120 °C, silicone is the only realistic option.
Pick by application, not price: heat and food contact favor silicone; abrasion favors TPU; cost favors TPE-S.

Three materials, three failure modes

Silicone is a thermoset: once cured, it will not re-melt, which is why it survives 200 °C continuous and does not leach plasticisers. TPU is a thermoplastic polyurethane — an engineering thermoplastic with outstanding abrasion and tear resistance but a narrower heat window and a tendency to yellow over time. TPE (TPE-S) is a styrenic thermoplastic elastomer, cheap and injection-friendly, but it softens above ~100 °C and absorbs stains and oils.

The three questions that settle the route

  1. What temperature does it meet? Above ~120 °C continuous, silicone is the only realistic option.
  2. What touches it? Food, skin or a baby’s mouth points to platinum-cured silicone with an FDA / LFGB report.
  3. Does it wear or does it flex? For a wear surface (a phone bumper, a roller), TPU may beat silicone; for a seal that must rebound for years, silicone’s compression set wins.

Head-to-head

PropertySiliconeTPE-STPU
Continuous temp-60–200 °C-40–100 °C-40–100 °C
Food contactFDA / LFGB (Pt-cure)Grade-dependentGrade-dependent
Stain resistanceExcellentPoorGood
Tear / abrasionModerateModerateExcellent
Clarity / yellowingExcellentYellowsYellows
Relative costMid-highLowMid

A real pattern we see: TPE parts pass inspection and still come back yellowed by month six, because the buyer specified "soft rubber" without naming the chemistry. Naming the material in the drawing prevents that.