Platinum-cure (addition-cure) silicone crosslinks without by-products, so it stays clearer, resists yellowing and passes food/medical grades more easily — but it costs more and is sensitive to catalyst poisons. Peroxide-cure silicone is cheaper and more tolerant of impurities but leaves acidic by-products that need post-curing, which is why it is avoided for food, skin and medical contact.
The chemistry decides the by-products
Peroxide curing uses an organic peroxide that decomposes at temperature into free radicals that crosslink the polymer. Those peroxide fragments leave acidic by-products (often organic acids) in the part, which is why peroxide-cured silicone is post-cured — baked again to drive off volatiles. Platinum (addition) curing uses a platinum complex catalyst and a hydride crosslinker; the reaction adds across a vinyl group and produces no by-products, so the part is cleaner out of the mold.
What the choice changes in practice
- Purity: platinum-cure is the default for FDA / LFGB food contact, baby products and medical parts.
- Clarity: platinum-cure stays water-clear; peroxide-cure can haze or yellow.
- Cost: platinum catalyst is expensive; peroxide compounds are 10–30% cheaper.
- Poison sensitivity: platinum catalyst is poisoned by trace sulphur, amines and some organics — so platinum-cure LSR must stay clean.
How CYES specifies it
For food-grade and medical LSR we run platinum-cured compounds (FDA 21 CFR 177.2600 / LFGB / USP Class VI / ISO 10993 as required), and we post-cure HCR parts as a standard step regardless of catalyst, then verify volatiles where a spec calls for it.