LSR (liquid silicone rubber) is a two-part liquid pumped into a heated, closed tool and cured in seconds — it wins on tolerance, thin walls and high volume but costs far more in tooling. HCR (high-consistency rubber) is a stiff, filler-loaded compound pressed in an open cavity — it wins on thick sections, large parts and low launch volumes, at the cost of dimensional consistency and more finishing labour. The whole decision follows from one physical difference: viscosity.
The difference is viscosity, and everything else follows
Both routes start with the same chemistry: polydimethylsiloxane chains that crosslink when a platinum catalyst meets a hydride. What separates them is how much filler the compound carries, and therefore how the material arrives at the mold. HCR — also sold as HTV — is a gum-like compound roughly the stiffness of stiff dough, delivered in slabs or strips, then cut, weighed and placed into an open cavity before the press closes. LSR is supplied as two low-viscosity A and B components, pumped, metered and mixed 1:1 at the machine inlet, then injected into a closed heated cavity.
That single difference in how material enters the tool drives every other number: cycle time, tooling construction, achievable tolerance, minimum wall, labour content and scrap rate. A typical LSR tool runs at 170–200 °C and cycles in 20–60 s; an HCR compression press cures in 60–180 s per shot.
Where LSR wins
- Tolerance: closed-cavity injection holds tighter dimensions; CYES holds cavity features to ±0.008 mm by CNC and ±0.005 mm on LSR shut-off surfaces.
- Thin walls: low viscosity fills features down to ~0.25 mm reliably.
- Automation: near-zero scrap in a cold-runner system and 3–5× faster cycling cut landed cost at volume.
- Cleanroom medical: LSR is the standard route for ISO Class 7 medical parts.
Where HCR wins
- Thick sections and large parts: big flat parts (baking mats, large gaskets) are impractical on LSR presses.
- Low launch volume: compression tooling is $500–$3,000 vs $3,000–$15,000+ for LSR, so HCR is the default under a few thousand pieces.
- Wider compound choice: HCR accepts more fillers and hardness grades for non-critical parts.
How to decide in one table
| Attribute | HCR / compression | LSR / injection |
|---|---|---|
| Tooling (simple part) | $500–$3,000 | $3,000–$15,000+ |
| Min practical volume | 100–500 pcs | 3,000–5,000 pcs |
| Cycle time | 60–180 s | 20–60 s |
| Tolerance (50 mm part) | ±0.15–0.25 mm | ±0.1–0.2 mm |
| Best for | Large parts, low MOQ | Precision, high volume, overmolding |