Short answer

Hardness sets the trade-off between conformability and recovery. Softer silicone (20–40 A) conforms to rough surfaces and seals at low squeeze but sets more over time; harder silicone (60–80 A) resists extrusion and holds shape under pressure but needs a flatter mating surface. Seals are usually 40–60 A; grips and overmolds 40–70 A.

Shore A hardness scaleDurometer scale with application bands.040608010020–40 Asoft gaskets40–60 Aseals60–70 Agrips / keys70–80 Aextrusionconformablefirm / resistantSofter conforms to rough surfaces; harder resists extrusion.
Hardness trades conformability against recovery: softer seals rough surfaces, harder resists extrusion under pressure.

What hardness actually changes

Shore A is a measure of how much the surface resists indentation. For sealing it maps to two behaviours: conformability (how well the material fills the microscopic gaps on a mating surface) and recovery (how fully it springs back after being compressed). Softer rubber seals a rougher surface with less clamping force; harder rubber needs a flatter, better-finished surface but resists extrusion through a gap under pressure.

Selection by application

Shore ATypical useWhy
20–40 AVery soft gaskets, cushioningMaximum conformability, low clamp force
40–50 AStatic seals, food lidsGood seal at low squeeze
50–60 ADynamic seals, O-ringsBalance of seal and recovery
60–70 AKeypads, grips, overmoldsFirm feel, resists tearing
70–80 AHigh-pressure, extrusion resistanceResists extrusion under pressure

Hardness, compression set and temperature

Hardness and compression set are related but not the same. A 50 A part and a 70 A part can have identical compression set at room temperature, but at 150 °C the softer grade typically sets more because the network has more free volume to relax. That is why a high-temperature seal is often specified at 60–70 A even when a softer grade would seal more easily. We measure hardness on a Shore A durometer and verify compression set per ASTM D395 on request.