Short answer

In LSR, sections down to about 0.25 mm fill reliably; in HCR compression, keep walls above 0.5–0.8 mm. The true limit is not fill — it is tear resistance and demolding: a very thin section may mold fine and then tear when the part is stripped. Thin walls also need a well-placed gate so the material fills before it starts to cure.

Minimum wall thicknessThin-section fill limits for LSR and HCR.LSR injectionHCR compressionfills ~0.25 mmshort flex features0.4–0.5 mm generalgate fills thin firstkeep above0.6–1.0 mm~0.5 mm flex minthick sectionsThe real limit is tear strength and demolding, not fill.
LSR fills down to ~0.25 mm, HCR stays above ~0.5–0.8 mm — the true limit is tear resistance, not fill.

Fill is not the limit — tearing is

Low-viscosity LSR can fill surprisingly thin sections, but a 0.2 mm membrane has almost no tear strength, so it rips during demolding or in use. The practical minimum is set by the part’s function: a living hinge or a thin flex section may tolerate 0.3 mm; a load-bearing wall should stay above 1 mm.

Practical limits by process

ProcessMin wall (general)Min wall (short flex feature)
LSR injection0.4–0.5 mm~0.25 mm
HCR compression0.6–1.0 mm~0.5 mm

Design rules for thin walls

  • Blend thickness changes: avoid a 0.3 mm wall next to a 5 mm boss — the abrupt step tears at the junction.
  • Place the gate to fill the thin section first, before the material cures.
  • Add a radius at every corner to stop tear propagation.
  • Specify a higher-tear compound (higher-tear LSR) if a thin flex feature must survive millions of cycles.