Short answer

Flash is the thin skin of material that squeezes into the parting line because silicone’s low viscosity lets it flow into any gap larger than a few microns. It comes from tool condition (worn shut-off edges), clamping force, venting and the process itself — and it is minimized by tight tooling, correct clamp tonnage and good part design, not just by trimming.

Flash at the parting lineLow-viscosity silicone flowing into the mold parting gap.mold closedlow-viscosity LSRflashflashSilicone flows into any gap larger than a few microns.Tight shut-off + clamp force + venting = thin, trim-able flash.
Low-viscosity silicone bleeds into the parting gap; flash is controlled by tight shut-off, clamp tonnage and venting.

Why silicone flashes more than thermoplastics

Silicone, especially LSR, has a viscosity closer to honey than to molten plastic. Under injection pressure it will flow into any gap at the parting line, around inserts, and through worn shut-off edges. Thermoplastics flash too, but their higher melt viscosity makes them more forgiving. This is why a silicone tool must hold its shut-off surfaces far tighter than a plastic tool.

The four causes, ranked

  1. Worn shut-off edges: a parting line that was tight at T1 opens up after thousands of shots.
  2. Insufficient clamp force: the press must hold the tool closed against injection pressure.
  3. Poor venting design: trapped air forces material sideways through the parting line.
  4. Geometry: very thin or very tall features make the tool harder to seal.

How CYES controls it

We hold LSR shut-off surfaces to ±0.005 mm, run adequate clamp tonnage, and design vents so air leaves without pushing flash outward. Where a customer needs a trimless part, we design the parting line and shut-off so the part can be de-flashed by cryogenic deflashing or a light tear-trim instead of hand cutting.