Platinum-cured silicone spans roughly −40 °C to 230 °C continuous, which is why it survives freezers, ovens, dishwashers and boiling water. Specify the actual service range on the drawing — "high temperature" is not a spec.
The silicon-oxygen backbone is what resists heat
Silicone keeps its properties across a wide band because its silicon-oxygen backbone is far more heat-stable than the carbon-carbon backbone of plastics and most rubbers. It stays flexible in a freezer, survives oven and dishwasher heat, and does not become brittle or melt the way plastics do. The practical continuous range for food-grade platinum-cured silicone is about −40 °C to 230 °C.
The evidence behind the claim
Material selection lives or dies on data. This is the measured record behind our Material Selection programs — the same data you can request during qualification.
- Material compliance: third-party tested by CTI against FDA 21 CFR 177.2600, LFGB §30/31, RoHS and REACH, with per-batch reports — so “food grade” or “medical grade” means a documented grade, not a claim.
- Process capability (Cpk): five documented studies — LSR-MED-007 (Cp 1.31 / Cpk 1.24), FVMQ-SEAL-010 (Cpk 1.32), LSR-MED-011 (Cpk 1.27), HTV-GASKET-014 (Cpk 1.34), LSR-MED-018 (Cpk 1.68) — reported against the 1.33 target.
- Mold & cavity accuracy: ±0.008 mm CNC, ±0.005 mm LSR shut-off / gate, ±0.003 mm mirror-EDM.
- Certifications: ISO 9001 (61120Q012) and ISO 13485 (04724Q10000602), numbers and scope published — originals under NDA.
- Cleanroom: ISO Class 7 — roughly 10× cleaner than a Class 100,000 line — per ISO 14644-1:2015, report CR-2026-0714.
See the full engineering evidence page →
What to watch for when you source
"High temperature" on a quote is meaningless without a number. We state the operating range per compound and post-cure every batch 4–6 hours at 200 °C so the part is stable at the top of its range. If a supplier cannot state a temperature range with a test reference, they are guessing — and your part is the experiment.
| Specification | Typical / range |
|---|---|
| Continuous range | −40 °C to 230 °C |
| Short peaks | Higher, briefly |
| Chemistry | Silicon-oxygen backbone |
| Post-cure | 4–6 h at 200 °C |
| Beats | Plastics, EPDM, NBR at extremes |
| Specify | Actual service range + cycles |