Short answer

LSR injection mixes two liquid components, injects them into a heated mold, cures in seconds, then post-cures. The precision comes from low viscosity plus controlled cure — verified by measured tolerance, not by the word "LSR" on a brochure. The measurable bar is Cpk 1.24–1.68 and ±0.008 mm cavity tolerance — documented, not claimed.

Four steps, each one a quality gate

The LSR process is mix → inject → cure → demold. The two parts mix in a static mixer, inject at low viscosity into a heated mold, cure in seconds, and eject cleanly — then every part gets a 4–6 hour post-cure at 200 °C to drive out volatiles for FDA and LFGB compliance. Because the process is automated and closed, contamination risk is low, which is why medical LSR runs in our ISO Class 7 cleanroom.

The evidence behind the claim

A process matters only if it produces repeatable results. This is the measured record behind our Manufacturing Process programs — the numbers you can request during qualification.

  • Mold & cavity accuracy: ±0.008 mm CNC-machined cavities (MAKINO 24,000 RPM), ±0.005 mm LSR shut-off / gate features, ±0.003 mm mirror-EDM fine details.
  • Process capability (Cpk): five documented studies — LSR-MED-007 (Cpk 1.24), FVMQ-SEAL-010 (Cpk 1.32), LSR-MED-011 (Cpk 1.27), HTV-GASKET-014 (Cpk 1.34), LSR-MED-018 (Cpk 1.68) — against the 1.33 target.
  • Material compliance: CTI-tested against FDA 21 CFR 177.2600, LFGB §30/31, RoHS and REACH, per batch.
  • Certifications: ISO 9001 (61120Q012) and ISO 13485 (04724Q10000602), numbers and scope published — originals under NDA.
  • Cleanroom: ISO Class 7 — roughly 10× cleaner than a Class 100,000 line — per ISO 14644-1:2015, report CR-2026-0714.

See the full engineering evidence page →

What to watch for when you source

The claim to verify is tolerance. We hold ±0.005 mm on gate and shut-off features and document the capability — LSR-MED-011 (Cpk 1.27, n=80) and LSR-MED-018 (Cpk 1.68, n=125). Ask any "LSR" supplier for a Cpk number on their last run; the silence is the answer.

SpecificationTypical / range
StepsMix → inject → cure → demold
Post-cure4–6 h at 200 °C
Precision±0.005 mm gate / shut-off
Cpk1.27 / 1.68 (documented)
CleanroomISO Class 7 (medical)
VolumeMedium to high