DFM Design Checklist

A pre-tooling checklist for buyers and engineers. Run your design past these ten decisions before you pay for steel — each one is where cost, lead time or quality is won or lost.

DFM checklistDecide the key items before tooling.Wall & fillMold & flowuniform wallmin 0.3 mm (LSR)thin → fasterthick → sink/voidgate positionweld-line controlventscold runnerDraft & ejectTolerance & shrinkdraft ≥ 0.5–1°undercutstexture depthejector layoutshrink 2–4 %parting lineflash toleranceCPK target
Run the DFM checklist before tooling: uniform wall, draft, gate position, venting, undercuts and shrinkage all decided up front.

1 · The ten decisions — check before you cut steel

Run your design past these ten points before tooling. Each one is a place where cost, lead time or quality is won or lost.

  1. Wall thickness. Keep walls uniform. LSR can fill down to 0.25–0.5 mm; a comfortable working range is 0.5–3 mm. Solid silicone (HCR) suits thicker sections. Step transitions at ≤1.5× and keep ribs at 0.5–0.6× the nominal wall so they don't sink.
  2. Gate position. Push air to a vent — position the gate so the flow front ends at a venting point, not a dead-end rib or boss. Hide the knit line on a non-cosmetic face.
  3. Mold venting. Typical vent depth is 0.01–0.03 mm, cut shallower on LSR (flashes through ~5 µm gaps). Plan vacuum-assisted venting for deep or trapped features.
  4. Draft angles. Add 1°–3° on vertical faces. Use 3°+ on deep cavities, tall ribs and textured surfaces. Flexible silicone can release many undercuts without a side action — if draft and geometry are planned for it.
  5. Undercuts & parting lines. Decide the parting-line placement early; specify where the flash line can sit on a cosmetic surface.
  6. Tolerances. Use generous tolerances where you can. Standard linear tolerance ±0.1–0.3 mm (size-dependent); mold cavities are machined to ±0.008 mm. Reference ISO 3302-1.
  7. Shrinkage & warpage. LSR shrinks 2.5%–3.5%, HCR 2.0%–3.0% by volume. The cavity is cut larger by the shrinkage factor; getting this wrong is why a first-article part measures out of spec.
  8. Overmolding. State the substrate material, surface treatment and bonding surface. Self-adhesive LSR bonds via silane coupling agents (no primer); ordinary LSR needs primer or plasma. Keep substrate withstand temperature 140–180 °C in mind.
  9. Fillets & radii. Add generous radii at sharp corners to reduce stress concentration and tearing on demold.
  10. First-article trial. T1 first shot — check fill, venting, knit lines and flash; confirm geometry against the drawing, then a dimensional report before release to production.

2 · Quick-reference numbers

ParameterLSR (liquid)Solid silicone (HCR)
Min / comfortable wall0.25–0.5 mm / 0.5–3 mmThicker sections
Volumetric shrinkage2.5%–3.5%2.0%–3.0%
Flash gapFlashes through ~5 µm gapsHigher viscosity, larger gap
Vent depth0.01–0.03 mm (shallower on LSR)
Draft1°–3° vertical faces; 3°+ deep cavities / textured
Standard tolerance±0.1–0.3 mm · mold cavities ±0.008 mm · ISO 3302-1

This checklist summarizes the full DFM design guide. Every DFM review at CYES is a written deliverable — a manufacturability report with risk and cost notes, not a phone call. Send your drawing and get a report back within 24 hours.

Common Questions

DFM Checklist FAQ

Sharp internal corners and uneven wall thickness cause tearing, voids and sink marks. Keep wall thickness uniform and use generous radii at transitions.
A typical minimum wall thickness is around 0.5–1.0 mm, depending on part size, material and flow length. Thinner walls can be molded but raise fill and tear risk.
Overmolding bonds silicone to plastic or metal in a single part and removes assembly labor. Choose it when a part needs a rigid core plus a soft sealing or gripping surface.

Need an Engineer's Answer for Your Exact Part?

Send your drawing — an engineer returns a written recommendation with samples.

Get a Free Recommendation

How we verify our claims.