Short answer

A self-adhesive LSR overmolded onto a primed PC, PA or metal substrate bonds stronger than the silicone itself — the failure is usually in the rubber, not the joint. Bond strength depends on substrate, primer and surface prep; PP and PBT are harder to bond chemically and may need mechanical interlock. Test the actual bond, because it is a process result, not a datasheet number.

Cohesive vs adhesive failureWhere the overmold bond breaks.Cohesive (good)Adhesive (weak)tears in the rubberinterface lets goA good bond fails in the silicone, not at the joint.
A good overmold bond fails cohesively (in the rubber); an adhesive failure at the interface means a weak bond.

Where the bond fails first

A good bond fails cohesively — the silicone tears, leaving a layer stuck to the substrate. An adhesive failure is the interface letting go cleanly, which means a weak bond. When you test, look at where it broke, not just the force number.

What drives the number

  • Substrate: PC and PA bond well; PP and PBT are low-energy and weak.
  • Primer + cleanliness: a primer and a clean, dry surface are decisive.
  • Cure conditions: the bond forms during cure, so temperature and time matter.
  • Geometry: holes, undercuts and knurling add a mechanical anchor.

How to verify it

Run a pull or peel test on the actual overmolded assembly, and confirm the failure is cohesive. Ask for a bond-strength report tied to your substrate and process, not a generic silicone datasheet.