Short answer

A 3× spread between silicone mold quotes is usually legitimate — and it is almost never about one factory being greedy. The gap is steel grade, cavity count, tolerance class, cold-runner vs open-runner, surface finish, and what each supplier assumed you didn't specify. The real risk is not the expensive quote; it is the cheap one that silently quoted the cheapest default and will hand you the difference later as flash, drift, or a mold that dies in 50,000 shots.

The quote gap is a specification gap

When a buyer sends "I need a silicone mold for a cup lid, about 60 mm" to three factories, they have not sent a mold specification — they have sent a guess. Each factory fills the blanks differently, and every blank is a cost lever. One quotes a two-cavity P20 tool with an open runner and a standard texture; another quotes a four-cavity NAK80 tool with a cold runner and a mirror polish. Both are "a mold for a 60 mm cup lid," and neither is lying.

The first thing to accept is that mold cost is not a commodity. It is a stack of decisions you are paying someone else to make for you if you don't make them yourself. The more precisely you specify, the closer the quotes converge — and the remaining spread tells you something real about capability and overhead.

The six levers that move a mold quote

Almost every meaningful price difference traces back to one of six things. None of them is optional; they are simply decisions with a cost attached.

  • Steel grade. P20 is the general workhorse; NAK80 and S136 are corrosion-resistant, high-polish steels for mirror finishes and cleanroom/medical work; hardened steels last far longer. A grade that isn't named on the quote is almost always the cheapest default.
  • Cavity count. Every additional cavity roughly repeats the machining cost. A four-cavity tool is not 4× a single cavity — but it is close to it for the machining, and the price jump is immediate.
  • Tolerance class. Holding ±0.05 mm on a critical dimension means slower EDM, more finishing, and more inspection. Loosen the tolerance and the cost drops; the part may no longer fit.
  • Cold runner vs open runner. A cold-runner LSR tool keeps the runner uncured so material is reused, but it adds manifold cost up front. An open runner is cheap but throws the runner away every shot.
  • Surface finish and texture. A mirror SPI A-1 finish or a deep, consistent texture is labor-intensive. A generic "fine matte" hides a lot of latitude.
  • Mold life warranty. A tool quoted for 500,000 shots in S136 costs more than one quoted for 50,000 in soft steel — and the per-shot economics flip entirely.

What the cheap quote is actually quoting

The danger in a mold quote is rarely that a supplier overcharges. It is that a supplier under-specifies to win the job and recovers the money later. The classic patterns:

  • The unnamed steel. If the quote doesn't say the grade, assume P20 or a soft equivalent — and expect earlier wear, more flash, and dimensional drift sooner.
  • The single-cavity default. Quoting one cavity when you need four makes the tool look cheap and the unit price look cheap — until you do the annual volume math and realize you need 4× the press time.
  • The "sampling included" trap. Some quotes bundle sampling; others charge for every trial shot. A low tooling number with per-trial fees is a loan, not a discount.
  • The ownership ambiguity. A factory that is vague about who owns the mold after you pay is often planning to keep quoting against "your" tool indefinitely.

This is why the cheapest quote can be the most expensive over a product's life. A mold that flashes, drifts, or needs a re-cut at 30,000 shots costs far more than the 2× you "saved" on tooling.

A side-by-side that exposes the gap

Here is how two honest quotes for the same nominal part can differ, and what each line actually buys you:

Line itemCheap quotePriced-for-production quote
Steel gradeP20 (unnamed, assumed)S136 / NAK80 (named)
Cavities14
RunnerOpen (scrap per shot)Cold runner (reuse material)
Tolerance±0.1 mm general±0.05 mm critical, controlled
FinishStandard matteMirror polish on A-surface
Expected life50,000 shots500,000 shots
Tooling priceLowHigher
True cost / partHigher (scrap, press time, rework)Lower over volume

Notice the inversion: the "expensive" tool is frequently the cheaper choice per finished part once volume, scrap, and rework enter the picture. Unit cost and tooling cost are two halves of one decision, not two separate ones.

How to force an apples-to-apples comparison

You don't need to become a tooling engineer to get comparable quotes. You need to stop sending a guess and start sending a spec. Five moves make the difference:

  1. Freeze the spec before you quote. Write down steel grade, cavity count, tolerance class, texture, and annual volume — then send the same sheet to every supplier.
  2. Demand a line-item breakdown. Tooling, sampling, and unit price should be three numbers, not one. The unit price is where the cheap tooling gets its money back.
  3. Ask for the steel by name. "What grade is the cavity in?" If the answer is vague, the default is the cheapest.
  4. Ask for expected shots and warranty. "How many shots is this tool good for, and what happens when it wears out before that?"
  5. Clarify ownership in writing. Confirm you own the mold, where it is stored, whether it is insured, and that you can transfer it. See our tooling payment terms and tooling, IP & NDA notes for the full picture.

One number we give buyers up front

When we quote a mold, we state the steel grade, the cavity count, the tolerance class, the runner type, the expected shot life, and the ownership terms in the quote itself — because those are the lines a buyer needs to compare us against anyone else fairly. If a quote you receive doesn't let you see those lines, that is itself information: you are being quoted a default, not a decision.