Most silicone parts fail for boring, preventable reasons: a plastic tolerance copied onto an elastomer, shrinkage discovered at trial instead of at CAD, a parting line across the sealing face. Below are the seven mistakes we see most often, a five-section DFM checklist to catch them, and the ISO 3302 standards that put numbers on the argument.
Why a failure list is more useful than a design guide
A design guide tells you what to do. A failure list tells you what goes wrong when you don't — and that is what actually saves a tooling budget. Every mistake below is one we have met on a real drawing, with the fix that would have avoided it. If you only read one section, read our ten-decision DFM checklist alongside this page; the two are complements, not duplicates.
The seven mistakes
1. Copying plastic tolerances onto an elastomer
A silicone part flexes, shrinks and moves in the mold. A ±0.05 mm tolerance across a 100 mm span — routine for injection-molded plastic — is often unachievable and, more importantly, unnecessary. Specify only the dimensions that affect fit or seal, and assign each one a realistic tolerance class. The framework is ISO 3302 tolerance classes, not a blanket number copied from a plastic print.
2. Discovering shrinkage at first trial
Silicone shrinks as it cures — broadly 1–3%, depending on grade, hardness and process. If shrinkage is only discovered when the first parts come out undersized, the tool usually needs re-cutting. Build compensation into the CAD from day one with our shrinkage calculator, then confirm the actual shrink factor on a trial run before committing to production steel.
3. Overusing undercuts
Every undercut either needs a side action — more steel, more cycle time, more cost — or a flexible part that can be demolded by hand. Designers often add undercuts for assembly convenience without pricing them. If an undercut is essential, flag it at the first DFM review so the molder can propose an alternate geometry or a split tool.
4. Running the parting line across the sealing surface
A parting line leaves a faint witness mark. On a sealing face, that mark is a leak path. Place the parting line away from any sealing-critical surface and say so on the drawing. This single decision prevents more field failures than almost any material choice — it is also covered in our sealing-parts guide.
5. Marking every dimension as critical
When everything is critical, nothing is. Marking twenty dimensions ±0.05 mm inflates inspection cost and can make a part uneconomic to produce. Separate the two or three sealing- or fit-critical dimensions from reference dimensions, and agree the measurement method for each. Our Cpk study shows how a real critical dimension is controlled.
6. Choosing material by hardness alone
Shore A is one number out of many. Tear strength, compression set, temperature range, food-contact or medical compliance and cure chemistry all matter, and two 50A grades can behave very differently in service. Start from the application and environment, then narrow the grade — the logic is in our material selector.
7. Letting the lowest mold quote decide cavity count
Cavity count is a production decision, not a tooling quote line. Too few cavities and the unit price never reaches target; too many and you pay for steel that idles. Balance annual volume, cycle time and press capacity before ordering steel. The trade-offs are worked through in mold cost breakdown.
The five-section DFM checklist
Run this before steel is cut. Each section is a question set your molder should be able to answer with you, not a box to tick alone.
| Section | Questions to settle | What a good answer sounds like |
|---|---|---|
| Material | Grade, hardness, shrinkage window, compliance needs? | A named grade with a stated shrink range and the exact reports available. |
| Geometry | Draft, wall thickness, radii, undercuts? | Uniform walls, adequate draft, undercuts priced or redesigned. |
| Tooling | Cavity count, parting line, mold steel? | Parting line off the seal; steel and life expectancy in writing. |
| Dimensions | Which dims are sealing-critical? Which tolerance class? | Two or three critical dims, each with an ISO 3302 class. |
| Production | Inspection method, post-cure, acceptance criteria? | Defined first-article inspection and a post-cure schedule. |
For the fuller ten-decision version, see DFM Design Checklist.
The standards behind the numbers
Tolerance arguments end quickly when both sides cite the same standard. ISO 3302-1:2014 (confirmed current in its 2024 review) defines rubber dimensional tolerance classes from Very Fine to Coarse. ISO 3302-2:2022 covers dimensional tolerances for rubber products after conditioning. For compression set, ASTM D395 is the common reference method. Cite the standard, the class and the dimension — not the word “tight”.
How CYES applies this
We run this checklist on every custom program before steel is ordered, and we return the results with the quote: grade recommendation, shrink factor, parting-line location, critical dimensions with tolerance class, and the inspection plan. It is the same engineering review behind our DFM guide and molding service. Send a drawing and we will mark the seven mistakes on it — free, before any tooling commitment.
Silicone vs engineering plastics — a DFM comparison
| DFM factor | Silicone (LSR / HCR) | Engineering plastics (PC, ABS, PA) |
|---|---|---|
| Typical wall thickness | 0.3–5 mm, flexible | 0.8–3 mm, rigid |
| Shrinkage (design in) | 1–3% depending on grade | 0.4–0.9% |
| Draft angle | 0.5–3°; bump-off often possible | 0.5–3°; no bump-off |
| Undercuts | Often demoldable by flexing | Need slides or lifters |
| Parting line | Keep off the sealing surface | Keep off the cosmetic face |
| Dimensional tolerances | ISO 3302-1 classes | ISO 20457 / DIN 16901 |
| Flash | Thin, from the parting line, removable | Rare with correct shut-off |
| Overmolding bond | Self-bonding LSR bonds chemically | Needs mechanical interlocks or adhesive |
Mold steel selection at a glance
| Steel | Best for | Notes |
|---|---|---|
| S136 (ESR) | High-polish, corrosion-resistant, medical/food | Mirror finish, longest life |
| NAK80 | High-polish, pre-hardened | Good polish, no heat-treat distortion |
| 718H / P20 | General-purpose production | Best cost/life balance |
| H13 | High-temperature or abrasive compounds | For hard or abrasive materials |
| Aluminum (7075) | Prototype / very short runs | Fast and cheap, limited life |