Silicone overmolding fails most often for one of two reasons: the bond does not hold, or the part warps. Selecting the right supplier is about verifying bond strength and substrate experience up front — not after the mold is cut. This is a selection checklist with the questions that separate a real overmolder from a molder that dabbles.

Cohesive vs adhesive failureWhere the overmold bond breaks.Cohesive (good)Adhesive (weak)tears in the rubberinterface lets goA good bond fails in the silicone, not at the joint.
Ask how a supplier proves bond strength — a cohesive failure in the rubber, not a peel at the interface, is the passing grade.
Cohesive vs adhesive failureWhere the overmold bond breaks.Cohesive (good)Adhesive (weak)tears in the rubberinterface lets goA good bond fails in the silicone, not at the joint.
Ask how a supplier proves bond strength — a cohesive failure in the rubber, not a peel at the interface, is the passing grade.

Why overmolding is a different discipline

Overmolding combines soft silicone with a rigid substrate — plastic or metal — in one part. It is a process, material and tooling challenge at the same time: the silicone must chemically or mechanically bond, the substrate must not deform, and the soft/rigid interface must hold dimension. A shop that only compression-molds silicone does not automatically know how to overmold it.

A 6-point checklist for selecting an overmolding supplier

  1. Substrate experience. Proven work with PC, ABS, PP, PA66, PBT and POM — not just "silicone overmolding" in the abstract. Ask for the specific resin you use.
  2. Bond-strength validation. Peel strength (N/mm) and lap shear (MPa), always named with substrate, silicone grade and bond route. A number without those three is not a measurement.
  3. Process route. Two-shot vs insert molding, chosen for your volume and geometry — not whatever machine is free.
  4. Pre-treatment and priming. A plan for surface treatment or primer where the substrate needs it to achieve a reliable chemical bond.
  5. Dimensional control. Measurement of the soft/rigid interface, with documented process capability where the part is critical.
  6. Design-for-overmolding. A DFM review that catches warping and bond risk before the mold is cut, not after.

How CYES measures up

Checklist itemCYES evidence
Substrate experienceOvermolding onto PC, ABS, PP, PA66, PBT and POM, plus metal inserts
Bond validationPeel and lap-shear testing on bonded samples, with substrate, grade and bond route documented per method
Process routesBoth two-shot molding and insert molding, selected for the application
Cleanroom optionISO Class 7 cleanroom for medical overmolded components
Quality systemsISO 9001 and ISO 13485 certified management systems

Overmolding & bonding guide · Bond strength testing · 2-shot overmolding guide

Questions to ask any overmolding supplier

How is silicone-to-plastic bond strength measured?
By peel strength (N/mm) and lap shear (MPa). A credible number always names the substrate, the silicone grade and the bond route.

Should I use 2-shot molding or insert molding?
It depends on volume, geometry and substrate — 2-shot for high volume with in-house substrate molding, insert molding for pre-molded plastic or metal inserts.

What substrates can be overmolded?
PC, ABS, PP, PA66, PBT and POM are common; some need pre-treatment or primer. Confirm proven experience with your exact substrate.

How do I avoid warping or bond failure?
Design-for-overmolding up front — gate location, wall thickness and thermal-expansion match — plus validated bond strength on your actual substrate and grade.

Request an Overmolding Review DFM Design Guide