Specify a trivet rated to 230 °C with a non-slip base and a Pantone-controlled finish — then verify the supplier with measured tolerance data and per-batch food-contact reports.
Heat rating and grip are the two numbers that matter
A trivet does two jobs: protect the counter from a hot pot and stay put while you set the pot down. Heat rating is a material spec — platinum-cured silicone spans −40 °C to 230 °C, so a hot cast-iron pan is fine. Grip is a base-texture and flatness problem: a trivet that rocks or slides is a mold defect, not a material one.
The evidence behind the claim
Before you approve a kitchen silicone tool, ask for the numbers behind the claim. This is the measured record we release for Kitchen & Cookware programs — the same capability and compliance data supplied at qualification.
- Material compliance comes first: food-contact grades are third-party tested by CTI to FDA 21 CFR 177.2600 and LFGB §30/31 — the two standards that actually gate cookware — with per-batch reports you can keep on file (RoHS/REACH included for any co-molded hardware).
- Process capability (Cpk): five studies we publish, not hide — LSR-MED-007 Cpk 1.24, FVMQ-SEAL-010 Cpk 1.32, LSR-MED-011 Cpk 1.27, HTV-GASKET-014 Cpk 1.34, LSR-MED-018 Cpk 1.68 — each reported against the 1.33 target with its sample size (n=50 to n=125).
- Mold & cavity accuracy: ±0.008 mm CNC cavities, ±0.005 mm LSR gate features, ±0.003 mm mirror-EDM details — the difference between a lid that seals and one that leaks.
- Certifications: ISO 9001 (61120Q012) and ISO 13485 (04724Q10000602), numbers and scope published — originals under NDA.
- Cleanroom: ISO Class 7 — roughly 10× cleaner than a Class 100,000 line — per ISO 14644-1:2015, report CR-2026-0714.
See the full engineering evidence page →
What to watch for when you source
Because it is a visible countertop product, color consistency and finish matter as much as function. We hold color to Pantone ±0.5 ΔE and control the base flatness so every trivet sits level. Our CNC-machined cavities hold ±0.008 mm, which is what keeps the texture crisp and repeatable across a run.
| Specification | Typical / range |
|---|---|
| Material | Platinum-cured silicone |
| Temperature | −40 °C to 230 °C |
| Base | Non-slip texture |
| Color | Pantone ±0.5 ΔE |
| Finish | Matte / ribbed / woven-look |
| MOQ | 500 pcs / SKU |