Specify a soft-durometer wrap with controlled surface tack, a graduated size set, and platinum cure — and verify the supplier with measured tolerance and per-batch FDA/LFGB reports, not just a "food-grade" label. The durometer here is Shore A 30 — ask for the measured range, not a catalog value.
Tack is the difference between a wrap and a mat
A reusable food wrap seals because of surface tack — a thin, slightly grippy surface that clings to a bowl rim. Too much tack feels sticky; too little and it will not seal. We control the surface finish and durometer (Shore A 30–50) so the wrap clings without being grabby, and cut a graduated size set so one package covers bowls, cut fruit and jars.
The evidence behind the claim
A datasheet can say “food-grade” in one line; the test reports take a little longer. Below is the measured record behind our Kitchen & Cookware programs — the same figures we put in front of a buyer during qualification.
- Material compliance comes first: food-contact grades are third-party tested by CTI to FDA 21 CFR 177.2600 and LFGB §30/31 — the two standards that actually gate cookware — with per-batch reports you can keep on file (RoHS/REACH included for any co-molded hardware).
- Process capability (Cpk): five studies we publish, not hide — LSR-MED-007 Cpk 1.24, FVMQ-SEAL-010 Cpk 1.32, LSR-MED-011 Cpk 1.27, HTV-GASKET-014 Cpk 1.34, LSR-MED-018 Cpk 1.68 — each reported against the 1.33 target with its sample size (n=50 to n=125).
- Mold & cavity accuracy: ±0.008 mm CNC cavities, ±0.005 mm LSR gate features, ±0.003 mm mirror-EDM details — the difference between a lid that seals and one that leaks.
- Certifications: ISO 9001 (61120Q012) and ISO 13485 (04724Q10000602), numbers and scope published — originals under NDA.
- Cleanroom: ISO Class 7 (ISO 14644-1:2015, report CR-2026-0714) for any run that touches skin or food.
See the full engineering evidence page →
What to watch for when you source
The defect to avoid is surface greasiness from low-grade plasticizer or peroxide residue. Specify platinum cure and request the LFGB §30/31 volatile report — a wrap that sits directly on food must clear volatiles, and that is exactly what our 4–6 hour post-cure step is for.
| Specification | Typical / range |
|---|---|
| Material | Platinum-cured food-grade silicone |
| Shore A | 30–50 (wrap body) |
| Surface | Controlled tack, non-sticky |
| Compliance | FDA 21 CFR 177.2600 · LFGB §30/31 |
| MOQ | 500 pcs / SKU |
| Temperature | −40 °C to 230 °C |